Applications Suitable for welding steel containing 22 - 26% Cr, 11 - 14 % Ni, 2 - 3% Mo, also for joints between 18 Cr, - 8 Ni, stainless steel and mild steel, or low alloy steel as well as clad steel.
Characteristics on Usage A low carbon stainless steel electrode for welding heat resistant Cr and Cr - Ni alloyed steel. It is a medium heavy coated rutile type, all position electrode yielding 25 Cr, 12 Ni, 2 Mo stainless steel weld deposit. The ferritic austenitic weld metal is very crack resistant smooth weld with clean edges. Suitable for welding build up turbine runners made of ferritic chromium stainless steel specially designed for welding root run in clad steel as well as mild steel.
Packing and Welding Current
SIZE ( mm ) |
KG PER PACKET |
KG PER CARTON |
Current (Amps) |
In Amps |
2.50 x 350 |
2 |
10 |
AC / DC (+) |
45 - 85 |
3.15 x 350 |
2 |
10 |
|
85 - 115 |
4.00 x 350 |
2 |
10 |
|
100 - 145 |
5.00 x 350 |
2 |
10 |
|
135 - 180 |